left-arrow
Search for words on this site: powered by FreeFind
right-arrow

Redux thickness on starboard rib flanges

Depth of Redux on rib

Depth of Redux on rib: 2007-11-16.

Nikon Coolpix 8400

Thickness of Redux on rib at BL39 after pre-bonding. Note that the recess for the skin stiffener has a slightly thicker layer than the rest of the rib.


Depth of Redux on rib

Depth of Redux on rib: 2007-11-16.

Nikon Coolpix 8400

Thickness of Redux on rib at BL54 after pre-bonding. Note that the Redux layer is slightly thicker towards the LE than the TE.


Depth of Redux on rib

Depth of Redux on rib: 2007-11-16.

Nikon Coolpix 8400

Thickness of Redux on rib at BL75 after pre-bonding. Note that the Redux layer is slightly thinner towards the LE than the TE.


Depth of Redux on rib

Depth of Redux on rib: 2007-11-16.

Nikon Coolpix 8400

Thickness of Redux on rib at BL127 after pre-bonding. Note how much thinner all along this is than the other ribs.

left-arrowgo to previous picture page notepadback to journal page notepad go to next picture page right-arrow
listgo to list of photo pages list

Return to Rowland's home page


This page last updated 2008-05-03. I try to make this page as accessible as possible, by adhering to HTML 4 standards. Valid HTML 4.01! Valid CSS!
I welcome comments on this website. However, because of the amount of spam it attracts, I no longer post a direct e-mail address on this page. Instead, please click here to contact me using my i-name =Rowland.Carson. You will have to confirm that the message is genuine before it will be sent on to me.